Mechanical Properties Metric English Comments
Tensile Modulus 1.99 GPa
288 ksi
chs 2 in/min; ASTM D638
Network Polymers NPS 90-0827 Polystyrene
Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc.
Tensile Modulus 1.99 GPa
288 ksi
ASTM D638
American Polymers API 650-21 Polystyrene
API 650-21 has been developed for injection molding applications that need a higher degree of toughness and gloss than conventional polystyrene. This polymer approaches ABS type properties.Applicat..