Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.44 GPa | 2820 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 19.44 GPa | 2820 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific) LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |