Polymer Property : Tensile Modulus = 280.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.931 GPa
280.1 ksi
ASTM D638
Resirene Resirene® 6220 High Impact Polystyrene
Features:Low FlowEasy ProcessingGood GlossHigh ElongationFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Extrusion/ ThermoformingDisposablesGPPS/HIPS BlendsRefrigerator PartsInformation p..