Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 28.4 GPa | 4120 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp OX95338 PPS LNP* Lubricomp* OX95338 is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.Thi.. |
|||
Tensile Modulus | 28.4 GPa | 4120 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp OX95338 PPS (Asia Pacific) LNP* Lubricomp* OX95338 is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.Thi.. |