Polymer Property : Tensile Modulus = 2791 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 19.24 GPa
2791 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA
LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized.