Polymer Property : Tensile Modulus = 27600 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 190 - 221 GPa
27600 - 32100 ksi
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head..