Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.87 GPa | 2737 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |