Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.79 GPa | 2725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
Tensile Modulus | 18.79 GPa | 2725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific) LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |