Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.189 GPa @Temperature 120 °C |
27.4 ksi @Temperature 248 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |