Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 27.4 GPa | 3970 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RC008 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RC008 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |