Mechanical Properties Metric English Comments
Tensile Modulus 0.186 GPa
27.0 ksi
1mm/min; DIN 53457
Advanced Elastomer Systems VistaFlex® 911-N Thermoplastic Rubber  (discontinued **)
Description: A colorable high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as fr..