Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.61 GPa | 2699 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Tensile Modulus | 18.61 GPa | 2699 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific) LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive.. |