Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 178 GPa | 25800 ksi | Typical epoxy composite property |
Hexcel® HexTow™ PV42/850 Carbon Fiber HexTow™ PV42/850 (HS-CP-3300) carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. This fiber has been designed for a.. |