Polymer Property : Tensile Modulus = 25.5 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.176 GPa
25.5 ksi
ASTM D638
3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..