Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 25.08 GPa | 3638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |