Polymer Property : Tensile Modulus = 234 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-400 1K HTA-7W EP01 Continuous Filament Carbon Fiber
Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 12K HTA-7C EP01 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 12K HTA-7C EP03 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 12K HTA-7C NS01 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 3K HTA-7C EP01 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 3K HTA-7C EP03 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 3K HTA-7W EP01 Continuous Filament Carbon Fiber
Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 6K HTA-7C EP01 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Modulus 234 GPa
34000 ksi
Toho Tenax Besfight® G30-500 6K HTA-7C EP03 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..