Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 23.51 GPa | 3410 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LX08411 PEEK LNP* THERMOCOMP* LX08411 is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added feature of this material is: Opaque. |