Polymer Property : Tensile Modulus = 23.45 GPa
Polymer Property :
Tensile Modulus =
23.45 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Modulus
23.45
GPa
3401
ksi
ASTM D-638
PlastiComp Complet® LCF15/LGF35 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber
Composite PelletsInformation provided by PlastiComp, Inc.