Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 220 GPa | 31900 ksi | |
Cytec Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |