Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 22.68 GPa | 3289 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific) LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |