Mechanical Properties Metric English Comments
Tensile Modulus 22.44 GPa
3255 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF008 PC
LNP THERMOCOMP* DF008 is a compound based on Polycarbonate resin containing 40% Glass Fiber.