Polymer Property : Tensile Modulus = 2199 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 15.16 GPa
2199 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66
LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 15.16 GPa
2199 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific)
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 15.16 GPa
2199 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific)
LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber.
Tensile Modulus 15.16 GPa
2199 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).
Tensile Modulus 15.16 GPa
2199 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton OV00A PPS
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.