Mechanical Properties Metric English Comments
Tensile Modulus 14.99 GPa
2174 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Tensile Modulus 14.99 GPa
2174 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Tensile Modulus 14.99 GPa
2174 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Tensile Modulus 14.99 GPa
2174 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Tensile Modulus 14.99 GPa
2174 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Tensile Modulus 14.99 GPa
2174 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..