Mechanical Properties Metric English Comments
Tensile Modulus 14.94 GPa
2167 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
Tensile Modulus 14.94 GPa
2167 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
Tensile Modulus 14.94 GPa
2167 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant.
Tensile Modulus 14.94 GPa
2167 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear..