Polymer Property : Tensile Modulus = 21.09 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 21.09 GPa
3059 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific)
Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN..