Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 207 GPa | 30000 ksi | |
Eagle Brass 200/201 Nickel Alloy, 1/2 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Tensile Modulus | 207 GPa | 30000 ksi | |
Eagle Brass 200/201 Nickel Alloy, 1/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Tensile Modulus | 207 GPa | 30000 ksi | |
Eagle Brass 200/201 Nickel Alloy, 1/8 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Tensile Modulus | 207 GPa | 30000 ksi | |
Eagle Brass 200/201 Nickel Alloy, 3/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Tensile Modulus | 207 GPa | 30000 ksi | |
Eagle Brass 200/201 Nickel Alloy, Annealed Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Tensile Modulus | 207 GPa | 30000 ksi | |
Eagle Brass 200/201 Nickel Alloy, Full Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Tensile Modulus | 207 GPa | 30000 ksi | |
Touchstone MetPreg™ Fiber Reinforced Aluminum MetPreg™ is a unique Fiber Reinforced Aluminum (FRA) material, a true metal matrix composite (MMC), that makes use of all traditional composite processing techniques. MetPreg has all the advantages.. |