Polymer Property : Tensile Modulus = 20.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.144 GPa
20.9 ksi
ISO 527
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate
Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy..