Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 20.87 GPa
3027 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 20.87 GPa
3027 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific)
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.