Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 20.57 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 20.57 GPa
2983 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66
LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow.
Copyright © lookpolymers.com All Rights Reserved