Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.24 GPa | 2936 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East) LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |