Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.139 GPa | 20.2 ksi | ISO 527 |
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in.. |