Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.968 GPa | 430.5 ksi | ISO 527 |
Ecomass® 1950TU76 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Polyamide (PA6/10)Very Good ToughnessInformation provided by Technical Polymers |