Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.86 - 2.90 GPa | 415 - 421 ksi | ASTM D638M |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |