Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.832 GPa | 410.8 ksi | ASTM D-638 |
Axiall 8266 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.832 GPa | 410.8 ksi | ASTM D-638 |
Axiall 8266 Rigid PVC, Extrusion, Natural Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.832 GPa | 410.8 ksi | ASTM D-638 |
Axiall 8266 Rigid PVC, Extrusion, White Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |