Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.782 GPa @Temperature -40.0 °C |
403.5 ksi @Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |