Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.37 - 2.49 GPa | 344 - 361 ksi | ASTM D638M |
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features.. |