Polymer Property : Tensile Modulus = 2.11 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.11 GPa

@Thickness 3.20 mm
306 ksi

@Thickness 0.126 in
1mm/min; ASTM D638
LG Chemical ALPHALAC SF510 HIPS
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
Tensile Modulus 2.11 GPa

@Thickness 3.20 mm
306 ksi

@Thickness 0.126 in
1mm/min; ASTM D638
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
Tensile Modulus 2.11 GPa
306 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 67001XXH PBT+PC
LNP* THERMOCOMP* 67001XXH is a compound based on PC + PBT resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added featu..
Tensile Modulus 2.11 GPa
306 ksi
1 mm/min
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry)
Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic..