Polymer Property : Tensile Modulus = 2.034 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.034 GPa
295.0 ksi
ASTM D638
Resirene Resirene® 6110 High Impact Polystyrene
Features:High ImpactEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityApplications:Injection MoldingTV CabinetsRemote ControlsToysInformation provided by US distributor Calsak Corporation.