Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.828 GPa | 2875.8 ksi | ASTM D-638 |
PlastiComp Complet® LCF30-PA12 Nylon 12, 30% Long Carbon Fiber Content Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 30% long carbon fiber reinforcementInformation provided by PlastiComp, I.. |