Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.77 GPa | 2867 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East) LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |