Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.135 GPa | 19.6 ksi | MD |
Kuraray HYBRAR® CF3 Mono Layer Cast Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |