Mechanical Properties Metric English Comments
Tensile Modulus 0.131 GPa
19.0 ksi
ASTM D638
3M Dyneon™ CC622 PTFE 10% Graphite Filled  (discontinued **)
Product Form: Black, pelletized free-flowing powder. Applications include bearings, ring seals.Data provided by Dyneon.
Tensile Modulus 0.131 GPa
19.0 ksi
1mm/min
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical