Polymer Property : Tensile Modulus = 1885.4 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.999 GPa
1885.4 ksi
1 % Sec; ASTM D638
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent ..
Tensile Modulus 12.999 GPa

@Temperature 22.8 °C
1885.4 ksi

@Temperature 73.0 °F
1% Secant; ASTM D638
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..