Mechanical Properties Metric English Comments
Tensile Modulus 129 GPa

@Temperature 23.0 °C
18700 ksi

@Temperature 73.4 °F
Hexcel® HexPly® F515 Epoxy Resin, TSR9120 Carbon Tape
Fiber: Toray® T700SInformation provided by HexCel