Mechanical Properties Metric English Comments
Tensile Modulus 12.9 GPa
1870 ksi
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled
Tensile Modulus 12.9 GPa
1870 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp RFL38 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL38 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 12.9 GPa
1870 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK
LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Tensile Modulus 12.9 GPa
1870 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding.
Tensile Modulus 12.9 GPa
1870 ksi
ASTM D638
Plenco 5118 Phenolic, Granular, Transfer Molded
PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio..
Tensile Modulus 12.9 GPa
1870 ksi
ISO 527
Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized
A chemically coupled 50% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Tensile Modulus 12.9 GPa
1870 ksi
ISO 527
Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized
A chemically coupled 50% long glass fiber reinforced natural polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Tensile Modulus 12.9 GPa
1870 ksi
ASTM D638
Plenco 1581 Polyester, Briquette, Transfer Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..