Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.75 GPa | 1849 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 12.75 GPa | 1849 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V8280 PBT+PET 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Tensile Modulus | 12.75 GPa | 1849 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |