Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.165 GPa | 1764.4 ksi | ISO 527 |
Polyram PlusTek PA310G8BK10 Nylon 6.6 for injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 40% Glass fiber reinforced Nylon 6.6 for injection molding applications. Approved and listed by NSF/ANSI 61 International.Information provided by Polyram. |