Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 121 GPa | 17500 ksi | |
Eagle Brass 194 HSM® Copper, 1/2 Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Modulus | 121 GPa | 17500 ksi | |
Eagle Brass 194 HSM® Copper, Annealed High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Modulus | 121 GPa | 17500 ksi | |
Eagle Brass 194 HSM® Copper, Extra Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Modulus | 121 GPa | 17500 ksi | |
Eagle Brass 194 HSM® Copper, Extra Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Modulus | 121 GPa | 17500 ksi | |
Eagle Brass 194 HSM® Copper, Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Modulus | 121 GPa | 17500 ksi | |
Eagle Brass 194 HSM® Copper, Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |