Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.662 GPa @Temperature -40.0 °C |
1691.4 ksi @Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)