Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.63 GPa | 2412 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX04489C PC LNP STAT-KON* DX04489C is a high modulus compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Con.. |